Dry Electrode Manufacturing Is Gaining Momentum — Why PTFE Fibrillation Matters

Removing the solvent is only half the challenge. The other half is making an electrode that can hold together without it.

Editorial visualization of electrode-roll manufacturing; conceptual imagery, not a photograph of Yonghe production.

Dry electrode manufacturing is attracting growing attention as battery producers seek ways to simplify production, reduce energy consumption, and manufacture thicker electrodes. By eliminating conventional solvent-based slurry coating and drying, dry processing offers a potentially more efficient route to lithium-ion battery production.

But removing the solvent also changes how the electrode must be assembled.

Without a conventional slurry-based binder system, active materials and conductive additives still need to form a cohesive, uniform film capable of surviving mixing, rolling, lamination, and electrochemical operation.

One of the most extensively studied solutions relies on an unusual property of polytetrafluoroethylene (PTFE): its ability to form microscopic fibrils under mechanical shear.

This process, known as PTFE fibrillation, is central to several leading dry electrode technologies. Yet controlling it is considerably more complicated than simply applying greater mechanical force. [1,2]

1. Why Dry Electrode Manufacturing Is Different

In conventional lithium-ion electrode manufacturing, active materials, conductive additives, and polymer binders are dispersed in a liquid to form a slurry. The mixture is coated onto a current collector, followed by drying and further processing.

While technically mature, this approach requires solvent management, drying equipment, and significant energy input. During drying, binder and conductive additives may also redistribute within the electrode, potentially affecting the uniformity of thick coatings. [1,3]

Dry electrode manufacturing aims to avoid these limitations by processing electrode materials without conventional slurry solvents.

Figure 1. Simplified comparison of conventional wet processing and a representative PTFE-based dry route. Processing sequences vary by technology; schematic only.

A typical PTFE-based route involves several interconnected stages: powder mixing, shear-induced fibrillation, film formation, calendering, and integration with a current collector. The exact sequence depends on the manufacturing technology.

Research by Oh et al., for example, separates the process into granule formation, film formation, pressing, and lamination, emphasizing the importance of understanding the material at every intermediate stage. [4]

Instead of relying primarily on a polymer distributed through a liquid slurry, the dry electrode needs a structure capable of mechanically connecting solid particles. That is where PTFE fibrillation becomes important.

2. How PTFE Fibrillation Holds an Electrode Together

PTFE is commonly associated with chemical resistance, thermal stability, and low surface energy. In dry electrode processing, however, its response to mechanical deformation is particularly valuable.

Under suitable shear conditions, certain PTFE powders can develop elongated, fiber-like structures. These fibrils extend through the powder mixture and form an interconnected network around active material and conductive additive particles. [1,3]

Figure 2. Conceptual depiction of how PTFE fibrils may link electrode particles under suitable shear. Not to scale; not an SEM image or measured result.

The resulting network provides mechanical cohesion, helping transform loose powder into a self-supporting electrode film. PTFE does not need to chemically bond every particle together; its fibrillar network physically entangles and supports the electrode components.

It is also important to distinguish mechanical cohesion from electrical conduction. PTFE is electrically insulating; electronic transport still depends on the active materials and conductive additives forming an effective conductive network.

Consequently, a mechanically strong electrode is not automatically an electrochemically effective electrode. The binder network must provide sufficient integrity without compromising the distribution and connectivity of the other components.

3. Why PTFE Fibrillation Is More Complicated Than It Looks

A PTFE powder does not fibrillate independently of its surroundings. Its behavior depends on the powder’s characteristics, the particles around it, and the mechanical history of the mixture. Recent research shows that these interactions can significantly influence the final electrode structure.

The Role of Conductive Carbon

In a 2025 study published in Energy & Environmental Science, Lee et al. investigated the formation of a dual-fibrous PTFE network in dry NCM811 cathodes. [3] Their findings highlight the importance of conductive carbon black in transferring shear forces to PTFE.

Carbon black can physically interact with the PTFE particle surface and facilitate fibril formation during kneading. Without sufficient interaction between the materials, PTFE may form poorly distributed aggregates rather than a uniform fiber network.

The researchers developed a staged process in which an initial portion of PTFE was fibrillated before grinding, followed by the addition of more PTFE and a second kneading step. This produced a combination of thin PTFE fibrils and thicker, rope-like structures.

For their specific formulation, the researchers used a final composition containing 3 wt% PTFE and 7 wt% carbon black. These values should not be interpreted as universal formulation recommendations.

The broader lesson is more important than the exact percentages: how PTFE is introduced and processed can be as important as how much PTFE is used.

Particle Size Changes How Shear Is Transferred

Active material particle size is another critical factor. A study published in Communications Materials investigated PTFE fibrillation using a multiscale framework combining finite element modeling, Gaussian process regression, and Bayesian optimization. [5]

The researchers demonstrated that particle size and the forces transmitted through particle contacts influence PTFE deformation. An appropriately designed bimodal particle-size distribution improved fibrillation under the studied conditions; other particle combinations resulted in insufficient or excessive deformation.

Two mixtures containing the same PTFE grade may therefore respond differently to the same equipment settings simply because their surrounding particles transmit mechanical forces differently. PTFE selection cannot be separated from the characteristics of the active material and conductive additives.

Mixing Time and Processing History Matter

Mechanical energy must be sufficient to initiate and develop a fibrillar network, but the relationship between processing intensity and electrode performance is not linear.

Hong et al. studied PTFE fibrillation in dry cathodes for all-solid-state batteries by varying kneading time from 10 to 120 minutes. Their work showed that optimizing fibrillation degree was important for balancing mechanical and electrochemical performance. [6]

Although the study focused on all-solid-state batteries, it illustrates a wider engineering principle: longer processing does not necessarily produce a better electrode. Mixing sequence, shear intensity, temperature, and the material’s condition before processing must all be considered.

4. More Fibrillation Does Not Always Mean a Better Electrode

One of the most important challenges in PTFE-based dry processing is determining when fibrillation is sufficient. Too little fibrillation can leave the electrode mechanically weak, with poor particle cohesion and an uneven binder network.

In the study by Lee et al., poorly developed PTFE structures were associated with rough electrode edges, reduced tensile strength, and cracking during subsequent processing. [3]

However, excessive processing introduces different problems. High mechanical stress can damage an established fibrillar network, create fragmented fibers, or cause localized material deformation. Active material particles may also be damaged by aggressive processing conditions.

Figure 3. Qualitative illustration of under-fibrillation, an appropriate processing window, and over-processing. Conceptual framework only; not experimental data.

Research on calendering provides a useful example. A 2026 study in the Journal of Manufacturing Science and Engineering examined dry NMC622 cathodes and found that calendering simultaneously influences electrode density, PTFE fibrillation, particle integrity, and porosity. [7]

Greater compression can improve particle contact, but excessive compression may fracture active material particles or reduce the pore structure needed for ion transport. The researchers identified a processing window that balanced competing requirements in their specific system.

The objective is not maximum fibrillation. It is the right fibrillar structure for the intended electrode formulation and manufacturing process.

5. The Real Test: Moving Beyond Laboratory Results

Producing a cohesive electrode sample in the laboratory is an important achievement. Reproducing that result consistently on a production line is a different challenge.

Industrial dry electrode manufacturing requires control over multiple variables at the same time. Powder flowability affects feeding consistency; mixing conditions influence fibril distribution; film formation and calendering determine thickness, density, and mechanical integrity; and lamination introduces further requirements for adhesion to the current collector.

A process that works with small laboratory batches may behave differently when material throughput, equipment geometry, and operating conditions change. This is why recent studies increasingly examine the individual steps of electrode manufacturing rather than evaluating only the finished electrode.

Oh et al. demonstrated a fabrication-scale solvent-free process and investigated how different PTFE types and concentrations affected intermediate materials and electrode performance. [4]

Meanwhile, Lee et al. reported a dual-fibrous dry electrode approach evaluated in 1.2 Ah-class pouch cells. In their graphite-based pouch-cell configuration, the researchers reported 80.2% capacity retention after 600 cycles. [3]

This result is specific to the reported electrode chemistry, formulation, cell design, and testing conditions; it should not be generalized to all PTFE-based dry electrodes.

For industrial evaluation, mechanical measurements alone are insufficient. Electrode films also need to be assessed for structural uniformity, adhesion, electronic transport, electrochemical performance, and process repeatability.

Ultimately, successful development of a dry electrode process requires coordinated optimization of the binder, conductive network, active material, and manufacturing equipment.

6. What This Means for PTFE Material Selection

For a material supplier or electrode developer, selecting PTFE for dry processing requires more than comparing conventional datasheet values.

A standard PTFE fine powder datasheet may provide information such as particle size, standard specific gravity, tensile properties, and other material characteristics. These parameters are useful for identifying and comparing materials, but they do not independently establish how a particular PTFE grade will fibrillate within an electrode formulation.

A more meaningful evaluation should consider several questions:

  • How readily does the PTFE develop fibrils under the intended mixing conditions?
  • How uniformly are those fibrils distributed throughout the electrode mixture?
  • Does the resulting film have sufficient strength and flexibility for subsequent processing?
  • How do binder content and fibrillation behavior affect the conductive network?
  • Can the process be reproduced consistently under the target manufacturing conditions?
  • Does the completed electrode meet the required electrochemical performance targets?

Depending on the development stage, these questions may be investigated through microscopy, mechanical testing, rheological or torque measurements, electrode resistivity, and cell-level testing. [3–7]

There is no reason to expect one PTFE grade or processing recipe to be optimal across every electrode chemistry and production method.

A Material Supplier’s Perspective

Yonghe manufactures Niflon® PTFE fine powders for industrial processing applications. Among its published grades, Niflon® SF-16T is a PTFE fine powder listed for paste extrusion and biaxially stretched film applications. [8]

Its potential use in dry electrode development would require formulation-specific evaluation. Published specifications for conventional processing applications should not be treated as evidence of qualified battery performance.

For customers investigating PTFE-based dry electrode technologies, material selection is best approached as a technical evaluation process involving powder characteristics, processing conditions, and the performance of the finished electrode.

7. Looking Ahead: From Fibrillation to Process Control

Dry electrode manufacturing has moved beyond demonstrating that PTFE can form fibers. The more demanding question is how to produce the appropriate fibrillar structure consistently, within a manufacturable processing window, and without compromising electrochemical performance.

Research is increasingly connecting microscopic deformation, powder interactions, processing parameters, and electrode-level results. [3–7]

This development points toward a more systematic approach to binder evaluation, where material properties and process conditions are investigated together.

For PTFE suppliers, that creates an opportunity to contribute beyond conventional resin specifications. Understanding powder behavior under relevant processing conditions may support more productive technical discussions with electrode developers and equipment manufacturers.

The future of PTFE-based dry electrode processing will depend not simply on forming fibrils, but on controlling where, when, and how they form.

 

EXPLORING PTFE FINE POWDERS FOR YOUR APPLICATION?

Yonghe offers Niflon® PTFE fine powder grades, including SF-16T, for industrial material applications and preliminary technical evaluation. If your team is investigating PTFE materials for dry electrode development, contact us to discuss available technical documentation and your specific material requirements.

Product information: https://www.yonghe-chemical.com/products/niflon-ptfe/

References

[1] Schumm, B.; Dupuy, A.; Lux, M.; Girsule, C.; Dörfler, S.; Schmidt, F.; Fiedler, M.; Rosner, M.; Hippauf, F.; Kaskel, S. (2025). Dry Battery Electrode Technology: From Early Concepts to Industrial Applications. Advanced Energy Materials, 15(24), 2406011. DOI: 10.1002/aenm.202406011. https://doi.org/10.1002/aenm.202406011

[2] Park, H.; Jin, C.; Daniel, C.; Li, J. (2026). Dry-Processed Electrodes Enabled by Polytetrafluoroethylene Fibrillation for High-Performance Lithium-Ion Batteries. Progress in Materials Science, 160, 101674. DOI: 10.1016/j.pmatsci.2026.101674. https://doi.org/10.1016/j.pmatsci.2026.101674

[3] Lee, K.-H.; Shim, H.; Lee, S. H.; Kim, H.-J.; Park, C.; Choi, J.; Lee, S.-J.; Hong, Y.-K.; Lyu, J.; Kim, J. C.; Park, S.; Cha, H.; Jin, W.; Kim, J.; Choi, S.; Lee, S.-Y.; Jung, S.-K.; De Volder, M.; Kim, T.-H.; Song, G. (2025). Dual-Fibrous PTFE Structure Enabling Uniform and Thick Dry Electrodes for High-Energy-Density and Long-Lasting Batteries. Energy & Environmental Science, 18, 8446–8461. DOI: 10.1039/D5EE03240G. https://doi.org/10.1039/D5EE03240G

[4] Oh, H.; Kim, G.-S.; Hwang, B. U.; Bang, J.; Kim, J.; Jeong, K.-M. (2024). Development of a Feasible and Scalable Manufacturing Method for PTFE-Based Solvent-Free Lithium-Ion Battery Electrodes. Chemical Engineering Journal, 491, 151957. DOI: 10.1016/j.cej.2024.151957. https://doi.org/10.1016/j.cej.2024.151957

[5] Kang, J. H.; Jeong, W.; Kang, M. S.; Kim, H. W.; Jeon, D. W.; Lee, H. U.; Hong, J. H.; Han, S.; Kim, M.; Yang, S.; Lee, D.; Kim, P. J.; Song, T.; Yoon, M.; Su, L.; Choi, J.; Cho, S. B. (2026). Multiscale Insights Enable Rational Design of Solvent-Free Dry Electrode Processing for Advanced Battery Electrode Fabrication. Communications Materials, 7, Article 34. DOI: 10.1038/s43246-025-01046-0. https://doi.org/10.1038/s43246-025-01046-0

[6] Hong, J.; Yoon, J.; Park, J.-W.; Ha, Y.-C.; Lee, J.; Hwang, I. (2025). Optimization of PTFE Fibrillation in Dry Electrode Process for Scalable All-Solid-State Battery Manufacturing. Journal of Power Sources, 655, 237925. DOI: 10.1016/j.jpowsour.2025.237925. https://doi.org/10.1016/j.jpowsour.2025.237925

[7] Park, H.; Jin, C.; Trask, S.; Jansen, A.; Li, J. (2026). Engineering Microstructure in Dry-Processed Cathodes Via Calendering. Journal of Manufacturing Science and Engineering, 148(10), 101002. DOI: 10.1115/1.4071854. https://doi.org/10.1115/1.4071854

[8] Yonghe. Niflon® PTFE — Product Specifications, Applications, and Storage and Handling Information. Official manufacturer product page. Accessed November 4, 2026. https://www.yonghe-chemical.com/products/niflon-ptfe/

Share :
Related News
Let's Have A Chat
CONTACT US